I. Hydraulic Pressure Test (Steam-Water Pressure System, Core Strength Test)
1. Timing of Test
After welding of heating surfaces, headers and pipelines is completed, NDT is qualified, and components requiring heat treatment have finished heat treatment; before thermal insulation, painting and refractory casting;
Required for new installation, major overhaul, large-area replacement of heating surfaces, restart after long-term shutdown, and when major defects are found during internal inspection;
Periodic inspection: once every 6 years under normal conditions; once every 3 years for boilers where internal inspection is not accessible.
2. Test Pressure (GB 50273-2022)
Drum boiler main body: 1.25 times the rated working pressure
Reheater system: 1.5 times the reheater working pressure
Steel tube economizer: 1.5 times the drum working pressure; cast iron economizer: 1.25 times drum pressure plus 0.5 MPa
Once-through boiler: 1.25 times the design pressure of the superheater outlet header, and not less than 1.1 times the pressure at the economizer inlet
Priority shall be given to the manufacturer’s drawings and technical agreement; if the drawing requirements are stricter than national standards, the drawing shall prevail.
3. Key Requirements for Medium, Temperature and Water Quality
Medium: clean demineralized water / softened water; chloride ion ≤ 25 mg/L for austenitic stainless steel tube bundles to prevent chloride-induced stress corrosion cracking
Ambient temperature ≥ 5 ℃; anti-freezing measures shall be taken if lower than 5 ℃
Water temperature: above dew point (to avoid misjudging external condensation as water leakage), ≤ 70 ℃; alloy steel shall be tested above the ductile-brittle transition temperature to prevent low-temperature brittle fracture
Water filling: keep all air vents fully open; close the vents only after steady water outflow without bubbles to completely vent air inside tubes and headers. Otherwise, pressure drop will be distorted and local air locking may cause overpressure.
4. Step-by-Step Pressurization Procedure (Mandatory)
1.Pressurize to 0.3~0.4 MPa: pause for preliminary inspection; bolts on flanges, manholes and handholes may be retightened (retightening is forbidden during the overpressure stage under pressure)
2.Continue pressurization to rated working pressure, hold pressure for full inspection, proceed to further pressurization only if no abnormality is found
3.Working pressure → test pressure: pressurization rate ≤0.2 MPa/min; rate ≤0.5 MPa/min before reaching working pressure; strictly avoid overpressure
4.Hold at test pressure for 20 min, record pressure drop
5.Reduce pressure slowly back to rated working pressure, and carry out careful leakage inspection at working pressure (welds, expanded joints, finned tubes, header nozzles)
Safety valves must be isolated (blind plate / clamping) and shall not participate in hydraulic test; main steam valves, feedwater valves and blowdown valves shall be tested together with the main body; local water level gauges are generally isolated and excluded from overpressure test.
5. Pressure Gauge Requirements
No less than 2 calibrated pressure gauges of the same range; range shall be 1.5~3 times the test pressure (2 times preferred); accuracy class ≥1.0 for high-pressure utility boilers.
6. Acceptance Criteria (GB 50273-2022)
1.No water droplets, mist or seepage on pressure-bearing components, welds and tube walls; slight dampness is acceptable for expanded joints but dripping is prohibited
2.No visible residual deformation
3.Pressure drop within allowable range specified by the code (classified by drum pressure: p<0.8 MPa ≤0.05 MPa; 0.8~1.6 MPa ≤0.1 MPa; 1.6~3.8 MPa ≤0.15 MPa; 3.8~9.8 MPa ≤0.3 MPa; ≥9.8 MPa ≤0.5 MPa)
7. Frequent Misconceptions of Hydraulic Pressure Test
❌ Misconception 1: Apply thermal insulation and paint before hydraulic test → leakage points will be covered and cannot be detected ❌ Misconception 2: Hold pressure without complete air venting → gas is compressible, leading to excessive pressure drop and false leakage judgment; local air locking may cause tube overpressure ❌ Misconception 3: Retighten bolts or enter hazardous areas for inspection under overpressure → severe safety risk; any leakage shall be handled only after full pressure relief ❌ Misconception 4: Use tap water directly for austenitic stainless steel without chloride control and fail to dry promptly after test → residual chloride ions will trigger stress corrosion cracking later ❌ Misconception 5: Hold pressure only for 10/15 min instead of 20 min; or inspect leakage directly at test pressure → the code requires leakage check after pressure drops to working pressure; tiny seepage droplets tend to evaporate under high pressure ❌ Misconception 6: Test without isolating safety valves → safety valves will pop and relieve pressure, resulting in test failure and potential damage to sealing faces ❌ Misconception 7: Low water temperature or ambient temperature below 5 ℃ without anti-freezing measures → water inside tubes freezes and bursts heating surfaces; external wall condensation is mistaken for leakage ❌ Misconception 8: Continuously replenish water to stabilize pressure when pressure drop exceeds limit → pressure must be relieved to check leakage or air lock instead of stabilizing pressure by water replenishment ❌ Misconception 9: Replace hydraulic test with air compression test for strength assessment → gas has high compression energy and explosion risk; air pressure strength test is strictly forbidden for boiler main bodies

II. Air Tightness Test (Tightness Test, Two Categories: Pressure-containing Medium Air Tightness / Furnace & Flue Gas Tightness)
Key distinction: Air tightness test ≠ air pressure strength test. Air tightness only checks micro-leakage and does not assess strength; it must be carried out after passing hydraulic strength test.
1. Application Scenarios
1.Gas-phase organic heat carrier furnaces (mandatory per GB 50273-2022);
2.Gas pipelines and gas valve assemblies of gas-fired boilers;
3.Furnace, flue, air duct and circulating flue gas system tightness test (often called air leakage test) for HRSG, CFB and incineration boilers;
4.Pressure pipelines carrying toxic or flammable & explosive media (trace leakage is not allowed).
Conventional steam boilers do not require air tightness test for steam-water systems, as hydraulic test covers tightness inspection.
2. Key Specification Points (Pressure-containing Air Tightness for Gas-phase Heat Carrier Furnaces)
Medium: dry clean air / nitrogen / inert gas; oxygen and combustible gas are prohibited; medium temperature ≥5 ℃
Test pressure: 1.05 times working pressure; all safety accessories shall be fully installed (opposite to hydraulic test)
Pressurization procedure: staged pressurization
Raise to 50% of test pressure → preliminary inspection
Then increase pressure step by step by 10% of test pressure, hold for 3 min at each stage
Hold for 10 min after reaching test pressure, then reduce to working pressure for point-by-point leakage inspection with foaming agent (soapy water)
Acceptance: no bubbles and no leakage; judgment shall not rely loosely on pressure drop indicators, as the core of air tightness is finding micro-leakage.
3. Furnace & Flue Tightness (Air Leakage Test, Negative Pressure / Slight Positive Pressure)
Commonly adopted for HRSG, CFB and incinerator flues: generally 300~500 mmH₂O (0.003~0.005 MPa), hold pressure for 10~15 min, pressure drop shall comply with design; measured by U-tube differential pressure gauge, soapy water for leakage check on welds, expansion joints, manholes, penetration seals and furnace wall gaps.
4. Frequent Misconceptions of Air Tightness Test
❌ Misconception 1: Reverse sequence, perform air tightness before hydraulic test → strength defects remain undetected and rupture may occur during air tightness test ❌ Misconception 2: Set air tightness pressure to 1.15 times (air pressure strength test pressure), excessive pressure → air tightness only checks leakage, not strength ❌ Misconception 3: Use humid air for air tightness; condensation in pipelines in cold weather makes foaming agent ineffective and leak points invisible ❌ Misconception 4: Safety valves, pressure gauges and transmitters are not fully installed or temporarily blocked during air tightness test → sealing status differs from actual operation and the test is invalid ❌ Misconception 5: Blow flues directly with high-pressure compressed air for air leakage test, damaging refractory materials and expansion joints ❌ Misconception 6: Only check pressure drop without point-by-point foaming inspection → tiny leakage (gas, heat transfer oil vapor) may cause negligible pressure drop and lead to fire or poisoning after commissioning ❌ Misconception 7: Combine gas pipeline air tightness and boiler main body hydraulic test into one system → gas system shall be isolated separately for independent air tightness test to prevent gas from entering steam-water system.
III. Comparison Table: Hydraulic Pressure Test vs Air Tightness Test
表格
Item Hydraulic Pressure Test (Strength Test) Air Tightness Test (Tightness Test)
Purpose Assess strength and macro tightness of pressure-bearing components Detect tiny permeable leakage, no strength assessment
Medium Water (demineralized / softened water) Dry air, nitrogen and other inert gas
Test Pressure 1.25 / 1.5 times working pressure (overpressure) 1.05 times working pressure (close to operating pressure)
Pressure Holding 20 min at test pressure, leakage check after pressure reduction to working pressure 10 min at air tightness pressure, foaming leakage check at working pressure
Safety Accessories Safety valves isolated with blind plates Safety valves and pressure gauges fully fitted
Main Risks Freezing, maintenance under pressure High gas energy storage; explosion risk for gas air tightness
Applicable Objects Boiler drum, water wall, superheater, reheater, economizer and other pressure-bearing heating surfaces Gas-phase heat carrier furnaces, gas pipelines, furnace and flue ducts
IV. General Management Guidance to Avoid Non-conformities (Most Frequently Raised by Inspectors)
1.Test procedure shall be prepared and approved, witnessed by supervisory inspectors; retrospective signature after test is prohibited
2.Clear isolation boundary for test system, blind plates with tags and isolation checklist
3.Post-test handling: drain and dry the boiler promptly after hydraulic test, and implement anti-corrosion preservation (wet preservation / nitrogen filling) to prevent internal corrosion; record air tightness test and close-loop recheck of all leakage points
4.Membrane wall and finned tube welds are high-risk leakage locations and shall be prioritized during hydraulic leakage inspection
5.For HRSG heat recovery boilers: flue air tightness test and tube bundle hydraulic test shall be performed separately and shall not be combined into one test

Share Post:

Related Products:

Boiler Fittings

The tube shield is a common component of the heating part of tubes. It is usually used in power station boilers. The useful life of

Read More »

Air Preheater

Air preheater(APH)is the shell and tube type heat exchangers used for preheating the air which is fed to the boiler or furnaces/ kilns for combustion

Read More »

Boiler water wall

Boiler water wall panels are a series of tubes welded together tangentially or with membrane bar between them to form the walls of the boilers

Read More »

Boiler Superheater

The Boiler Superheater is a coil type heat exchanger which is used to produce superheated steam or to convert the wet steam to dry steam,

Read More »

Boiler Steam Drum

The steam drum stores the steam generated in the water tubes and acts as a phase-separator for the steam/water mixture. Steam is separated from the

Read More »
Stay Connected

Latest Blogs